+86-312-6775656

Principles and Common Problems of Transformer Field Test Projects

Feb 19, 2024

1. What is the principle of diagnosing internal faults in transformers based on chromatographic analysis data of transformer oil?

The insulation of power transformers is mostly composed of oil-paper composite insulation. The hydrocarbon gases generated by internal latent faults come from the thermal cracking of oil-paper insulation. The gas production rate, gas production rate, and unsaturation of hydrocarbon gases generated by thermal cracking depend on the energy density of the fault point. The nature of the fault is different, the energy density is also different, and the hydrocarbon gas produced by cracking is also different. Corona discharge mainly produces hydrogen, arc discharge mainly produces ethylene, and high-temperature overheating mainly produces ethylene.

The energy at the fault point varies, and the rate of gas generation for the aforementioned gases also varies. This is because in the chemical structure of hydrocarbons such as oil paper, the bond energy of various bonds varies due to the different chemical bonds between atoms. Hydrocarbons with different chemical bond structures have varying degrees of thermal stability. Therefore, it is concluded that the order in which insulating oil decomposes to generate hydrocarbons as the temperature of the fault point increases is alkanes, olefins, and fast hydrocarbons. Additionally, since each hydrocarbon gas generated by oil cracking has a specific temperature range corresponding to the maximum gas production rate, it is derived that insulating oil produces different components under different fault properties of transformers Simple criteria for hydrocarbon gases with different concentrations.


2. Why does a slight impurity in the insulating oil cause a significant decrease in its breakdown voltage?

Take transformer oil as an example to illustrate this phenomenon. In transformer oil, there are usually bubbles (a common impurity), and the dielectric coefficient of transformer oil is more than twice that of air. Due to the inverse relationship between electric field strength and dielectric constant, and the distortion of the surrounding electric field caused by bubbles, the internal electric field strength in the bubbles is also more than twice that of transformer oil, and the electric field strength around the bubbles is higher. The electrical strength of gas is much lower than that of transformer oil.

So the bubbles in transformer oil are easily free. The charged particles generated after bubble dissociation collide with the molecules of oil, which then decompose into gas. Due to this chain reaction, also known as a vicious cycle, the gas growth will become faster and faster. Finally, the bubbles will arrange in rows along the direction of the electric field in transformer oil, ultimately leading to breakdown.

If the transformer oil contains water droplets, especially fibers with moisture (cotton yarn or paper), the insulation strength of the insulation oil will be most severely affected. Although there are few impurities, due to the chain reaction that can form through defects, the discharge voltage of the insulating oil will decrease significantly.

 

3. Why can the no-load test of transformers detect defects in the iron core?

The no-load loss is basically the sum of the hysteresis loss and eddy current loss of the iron core, with only a small portion being the resistance loss formed by the no-load current flowing through the coil. Therefore, the increase in no-load loss mainly reflects the defects in the iron core. The insulation paint quality between female silicon steel sheets is poor, and the deterioration of the paint film causes short circuits between silicon steel sheets, which may increase no-load losses by 10% to 15%; Insulation damage to parts such as core bolts and drive iron beams can increase eddy currents in the iron core, causing local heating and increasing overall no-load losses.

In addition, the use of silicon steel sheets thicker than the design value or of poor quality during the manufacturing process, as well as large gaps in the magnetic circuit joints of the iron core, can also increase no-load losses. Therefore, the measured losses can reflect the defects in the iron core.